Fine grain aluminum nitride castable with high thermal conductivity. Cure: Step 1. Dry for 8 hours minimum at room temperature. Step 2. Bake at 200 ºF for 2–4 hours. Step 3. Final cure at 250 ºF for 3 hours. Step 4. Final cure at 450 ºF for 30–60 minutes if using HLB-1 Hydrophobic Liquid Binder. |
Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |