MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1701 E (SEP) Linear Diblock Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1701 E is a clear linear diblock copolymer based on styrene and ethylene/propylene, S-E/P, with bound styrene of 35% mass. It is supplied from Europe in the product form identified:
Kraton G1701 EU - supplied as an undusted fluffy crumb

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1701 E is used in formulating adhesives and coatings, as base material for compound formulations, as a modifier of thermoplastics and as base material for oil gel applications. The inherent stability of the mid block suggests the use of this grade in applications that must withstand weathering and high processing temperatures.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Packaging and Polymod; and Personal Care

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccISO 2781
Volatiles <= 0.50 %KM 04
 
Descriptive Properties
ContentAntioxidant>0.03%, KM 08
 Polystyrene33.2-36.6%, KM 03

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® FG1901 G (SEBS) grafted with MA
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton® G1701 M (SEP) Linear Diblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer

PKRA9901 / 132800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.