MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Shin-Etsu Silicones X-30-783U Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics.

Product Features:

  • A broad range of service temperatures from 100 to +260°C (148 to +500°F.)
Typical Applications:
  • Low temperature gaskets.
  • Low temperature packing.

Information Provided by Shin-Etsu Silicones of America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.17 g/cc1.17 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4848
Tensile Strength at Break 12.94 MPa1877 psi
Elongation at Break 594 %594 %
Tear Strength 34.4 kN/m196 pliDie B
Compression Set 23 %
@Temperature 180 °C,
Time 252000 sec
23 %
@Temperature 356 °F,
Time 70.0 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -100 °C-148 °F
 
Descriptive Properties
Cure AgentDBPH
Cure TypePress Cure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-1052A/B Silicone, Gel RTV
Shin-Etsu Silicones LIMS™ KE1950-70A/B Elastomer
Shin-Etsu Silicones SV-18000U Silicone Rubber
Shin-Etsu Silicones SV-58000U High Strength Silicone Elastomer
Shin-Etsu Silicones FE-371U Fluorosilicone Elastomer

PSHIN268 / 177779

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.