MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsui APEL™ APL8008T Cyclo Olefin Copolymer (COC)
Categories: Polymer; Thermoplastic; Cyclo Olefin Polymer

Material Notes: This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt processability/flowability, good clarity and transparency, high glass transition temperature (Tg), exceptional moisture impermeability, impressive gas barrier qualities and excellent chemical and heat resistance. This material is used in Film Sheet applications.

Information provided by Mitsui Chemicals America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/ccASTM D792
Moisture Vapor Transmission 0.0900 cc-mm/m²-24hr-atm1 atm; ASTM D1249
Linear Mold Shrinkage 0.0060 cm/cmMCI Method
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPaASTM D638
Elongation at Break 100 %ASTM D638
Flexural Strength 90.0 MPaASTM D790
Flexural Modulus 2.40 GPaASTM D790
Izod Impact, Notched 45.0 J/mASTM D256
Izod Impact, Unnotched (ISO) 33.0 kJ/m²ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 °CTMA; MCI Method
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CASTM D648
Glass Transition Temp, Tg 70.0 °CMCI Method
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.54ASTM D542
Haze 2.0 %ASTM D1003
Transmission, Visible 91 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui APEL™ APL6015T Cyclo Olefin Copolymer (COC)
Mitsui APEL™ APL6013T Cyclo Olefin Copolymer (COC)
Mitsui APEL™ APL6011T Cyclo Olefin Copolymer (COC)
Mitsui APEL™ APL6509T Cyclo Olefin Copolymer (COC)
Mitsui APEL™ APL5014DP Cyclo Olefin Copolymer (COC)

PMIT138 / 53296

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.