MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M9.6GF Epoxy Resin Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M9.6GF is a hotmelt, thermosetting, moderate tack epoxy resin matrix, specifically designed for prepreg applications at which short cure cycles of 100°C and above are required. M9.6GF can be used for the manufacture of large industrial components and is suitable for the cure of thin and thick sections. M9.6GF exhibits a long out-life at ambient conditions.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 - 1.22 g/cc0.0397 - 0.0441 lb/in³
Viscosity  100 cP
@Temperature 105 °C
100 cP
@Temperature 221 °F
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 1000 cP
@Temperature 121 °C
1000 cP
@Temperature 250 °F
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 100000 cP
@Temperature 40.0 °C
100000 cP
@Temperature 104 °F
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 1.00e+6 cP
@Temperature 130 °C
1.00e+6 cP
@Temperature 266 °F
Dynamic Complex Viscosity of HexPly® M9.6GF @2°C/min
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 105 - 115 °C221 - 239 °FTypical cured, following a 30min cure @120°C
 120 - 130 °C248 - 266 °FOptimum cured, following a 120min cure @120°C
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 120 °C
0.500 hour
@Temperature 248 °F
+/-7min
 45.0 min
@Temperature 110 °C
0.750 hour
@Temperature 230 °F
+/-10min
 70.02 min
@Temperature 100 °C
1.167 hour
@Temperature 212 °F
+/-15min
Shelf Life  2.00 Month
@Temperature 23.0 °C
2.00 Month
@Temperature 73.4 °F
 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
 18.0 Month
@Temperature -18.0 °C
18.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
ColorOff white - Yellowish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9131 / 322287

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.