MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 6280 High Density Polyethylene, Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Characteristics:
  • Excellent stiffness
  • Excellent surface appearance
  • Good warp resistance
  • Excellent impact resistance
  • ASTM D 1248 - Type III, Class A, Category 3
  • FDA Compliant

Applications:

  • Dairy crates
  • Pallets
  • Material handling containers
  • Totes
  • Trays
  • Suitable for food packaging

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.962 g/ccASTM D792
ESCR 10% Igepal® >= 10 hourASTM D1693, Cond. B
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 4800 psiASTM D638
Elongation at Break 300 %ASTM D638
Flexural Modulus 230000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 265 °FASTM D3417
Brittleness Temperature -112 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 500 °FInjection Molding
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade
Bamberger Polymers Bapolene® 3257U Polyethylene, Injection Molding
Global V-1160 High Density Polyethylene, Injection Molding Grade
NOVA Chemicals SCLAIR® 2712CC HDPE Injection Molding Resin

PTOTAL746 / 130471

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.