Telcar TL-8730A is a high performance flame retardant thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a high density, higher hardness, UL 94 V-0 grade that is UV stabilized and RoHS compliant. This grade is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Brominated; Filled; Flame Retardant; Good Colorability; Good Electrical Properties; Halogenated; Heat Aging Resistant; High Elongation; High Tensile Strength; High Density; High Hardness; Low Temperature Flexibility; Medium Flow; Sunlight Resistant (720 hrs); UV Resistant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flame Retardant Insulation; Flame Retardant Jacketing; Flexible Cord Jacketing; Industrial Cable Insulation; Industrial Cable Jacketing; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing RoHS Compliant:RoHS Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |