High efficient stabilizer/lubricant one-pack based on Ca/Zn/Mg compounds in addition organic co-stabilizers.Imparts very good elecrtical insulation resistance and long term heat stability as well as the color hold in white pigmented formulations. Information provided by Pau Tai Industrial Corp. |