Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics, sound and vibration dampening, improved impact resistance, and U.V. stability. Elastocon® STK70 can be overmolded to polycarbonate, ABS, PC/ABS, Acrylic, HIPS, and various grades of nylon 6 and 6/6.Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics. |