MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terluran® HD-15 ABS
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes:

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Melt Flow 15.75 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 38.0 MPaISO 527
Elongation at Break 10 %Nominal; ISO 527
Tensile Modulus 2300 MPaISO 527
Izod Impact, Notched (ISO) 16.0 kJ/m²ISO 180
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 170 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179
 14.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 100 Hz
IEC 60250
Dielectric Strength 37.0 kV/mm
@Thickness 1.50 mm
K20/P50; IEC 60243-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 95.0 µm/m-°C
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °CISO 75
Vicat Softening Point 100 °CISO 306
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-22 ABS
INEOS Styrolution Terluran® HI-12 ABS
INEOS Styrolution Terluran® EGP-7 ABS
INEOS Styrolution Terluran® GP-35 ABS
INEOS Styrolution Terluran® HH-112 Q109 ABS

PBASG0612 / 132245

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.