MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VP Disp. ITO LTH2 Conductive lacquer
Categories: Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Thermal curable solvent based lacquer system with nanostructured Indium Tin Oxide for the production of electrical conductive, antistatic, transparent coatings on glass and polymer substrates such as PLEXIGLAS® (PMMA), PC, PET or TAC. Information typical of products used for flexible electronics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 30 %Indium Tin Oxide (ITO)
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 500 ohm - 1e+05
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 88 %
 
Processing PropertiesOriginal ValueComments
Cure Time 3600 sec
 
Descriptive Properties
Conductive Filler TypeIndium Tin Oxide (ITO)
Material TypeDispersion
Recommended SubstratesGlass PLEXIGLAS® (PMMA) PC PET TAC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VP Disp. ITO TC8 Coating
Evonik VP Disp. ITO LRC Conductive lacquer
Schott Transparent ITO Conducting Oxide Coating
Evonik VP Disp. ITO IR5 Coating
Evonik DEGALAN® VP 4240 D Methacrylic Polymer

PFLEXCM58 / 179460

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.