MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman BMC 6605A Polyester Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 g/cc
Water Absorption <= 0.10 %24 hours, 23°C
Linear Mold Shrinkage 0.0013 - 0.0035 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 23 - 25
Tensile Strength, Ultimate 7000 - 9000 psi
Flexural Strength 15000 - 20000 psi
Compressive Strength 20000 - 25000 psi
Izod Impact, Notched 3.00 - 5.00 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 400 - 440 V/milShort Time
Arc Resistance >= 180 sec
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 400 °F
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Mold Temperature 220 - 280 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® UP 3420 Unsaturated Polyester Resin, High Mechanical Strength, High Arc Resistance, UL Listed, Low Shrinkage
Westlake EM1550AA Low Density Polyethylene
Celanese Ateva® 2803G Ethylene Vinyl Acetate Copolymer
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer
IDI Composites Dielectrite® 48-50 Thermoset Polyester, Molding

PBMC026 / 27209

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.