MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Barlog Plastics KEBAFORM C 902 CF POM Copolymer, carbon fiber reinforced, electr. conductive
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: POM-CF10

Information provided by BARLOG plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527-1
Elongation at Break 4.0 %ISO 527-1
Tensile Modulus 6600 MPaISO 527-1
Charpy Impact, Notched 4.50 kJ/m²ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+05IEC 60093
Surface Resistance 10000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Melting Point 166 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
Resin TypePOM-CF10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei TENAC™-C CF452 Copolymer Acetal (POM), Medium Viscosity, Carbon Fiber Reinforced
Avient Edgetek® PC-10CF/000 Polycarbonate (PC), Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced
Avient Lubri-Tech™ PC-05CF/15T Polycarbonate (PC), Carbon Fiber Reinforced, PTFE Lubricated

PBARLO827 / 149845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.