MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: High clarity plastic for a multitude of applications
    Features
  • Clear and transparent
  • Rigid and tough
    • Great for headlamps, bottles and transparent assemblies
    • Excellent humidity/moisture resistance

    All information provided by 3D Systems.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
@Temperature 25.0 °C
Liquid
 1.15 g/cc
@Temperature 25.0 °C
Solid
Water Absorption 0.38 %ASTM D 570-98
Viscosity 180 cP
@Temperature 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 86
Tensile Strength 38.0 - 42.0 MPaASTM D638
Elongation at Break 10 - 22 %ASTM D638
Tensile Modulus 1940 - 2250 MPaASTM D638
Flexural Strength 73.0 - 76.0 MPaASTM D790
Flexural Modulus 1940 - 2250 MPaASTM D790
Izod Impact, Notched 23.0 - 51.0 J/mASTM D256
Penetration 7.2mils penetration depth
 
Thermal PropertiesOriginal ValueComments
CTE, linear 97.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
ASTM E 831-93
 216 µm/m-°C
@Temperature 70.0 - 140 °C
ASTM E 831-93
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 41.0 °CASTM D648
Glass Transition Temp, Tg 56.0 °CDMA, E"
 
Descriptive Properties
AppearanceClear
Critical Exposure (Ec)10.6 mJ/cm²

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® VeroBlack PolyJet™ FC870 for Rapid Prototyping
Stratasys® PolyJet™ TangoBlack™ FC970 Rapid Prototyping Material
DSM Somos® NanoTool™ Resin for Stereolithography, UV Postcure
3D Systems RenShape® SL 7820 Stereolithography Plastic
DSM Somos® NeXT Stereolithography (SLA) Prototyping Polymer

PAPPR115a / 176025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.