Hostacom ERC 1122N C12616 is a 15% talc filled PP copolymer, with good flowability, high stiffness, excellent scratch resistance and low emissions. The product is available as a customized color matched, pellet form. This grade is delivered in C12616 jet-black color version. Applications: Interior TrimsInformation provided by LyondellBasell. |