MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Acerde Tungsten
Categories: Metal; Nonferrous Metal; Refractory Metal; Tungsten Alloy; Pure Element

Material Notes: Tungsten key properties: Very high density, High oxidation resistance, Highest melting point of all metals, Lowest vapor pressure of all metals, Highest elasticity modulus of the all metals, Hardest pure metal, Excellent high temperature strength characteristics, High hardness, Resistive to thermal stress, High thermal conductivity, Low thermal expansion, Superior chemical inertness, is not attacked by nitric, hydrofluoric, or sulphuric acid solutions

Tungsten main applications domains: Inert gas welding electrodes, Metal evaporation work, X-ray targets, Windings and heating elements for electric furnaces, Electroplating, As tungsten yarn, it is used for reinforcement in metal, ceramic and plastic composites

Information provided by Acerde

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 19.25 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 411 GPa
Flexural Strength 610 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000530 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µm/m-°C
@Temperature <=1000 °C
Melting Point 3422 °C
 
Component Elements PropertiesOriginal ValueComments
Tungsten, W 100 %Impurity level not reported

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Transfer Composites PRIMEX™ MCX-693™ Aluminum Silicon Carbide Composite, Reinforced
Morgan Advanced Ceramics Mac-35 Au/65 Cu-WM Braze Alloy
Morgan Advanced Ceramics Nioro™ Mac-Nioro™-WM Braze Alloy
Morgan Advanced Ceramics 50Au-50Cu Mac-560Au/50 Cu-WM Braze Alloy
Morgan Advanced Ceramics Cusil™ Mac-Cusil™-WM Braze Alloy

CZACERD02 / 122020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.