MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco DEXRON®-III/MERCON® Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: General Description

DEXRON® is a specification for General Motors vehicles, but many foreign manufactures specify a DEXRON approved ATF as well. DEXRON-III can be used in transmissions that call for DEXRON-IIE or DEXRON-II.

Most Ford vehicles manufactured between 1980 and 1999 specify a MERCON ATF. ATFs that meet DEXRON-III requirements usually meet the MERCON requirements as well.

Chevron ATF DEXRON®-II/MERCON® is DEXRON®-III and MERCON® approved and is formulated with special base oil for exceptional protection from heat, oxidation and wear.

Applications

Chevron Automatic Transmission Fluid DEXRONIII/MERCON is designed for use in General Motors Corporation transmissions that specify a DEXRON-!!!, DEXRON-II fo DEXRON-IIE fluid and Ford Motor company transmissions that require a MERCON fluid.

It is an excellent choice in any transmission where the manufacturer recommends a DEXRON or MERCON qualified product. It is suitable for use in Mercedes Benz passenger car automatic transmissions and Voith and ZF truck transmissions.

It is also recommended for transmissions, power steering systems, and hydraulic systems requiring a DEXRON-III, Allison C4 or Caterpillar TO-2 fluid.

Chevron Automatic Transmission Fluid DEXRON-III/MERCON is also used as a light oil in compressors, pumps, and hydraulic systems.

Key Words: CPS Number: 226502; MSDS Number: 0021
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 32.7 °
Brookfield Viscosity 17000 cP
@Temperature -40.0 °C
Viscosity Measurement 172Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 180 SUS
Saybolt Viscosity at 210°F 50.3 SUS
Kinematic Viscosity at 40°C (104°F) 35.5 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.2 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °CASTM D97
Flash Point 202 °CASTM D92
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
Lubriplate DEXRON III / MERCON Automatic Transmission Fluid Motor Oil & Transmission Fluid
Water, H2O
Phillips 66 Dexron® -VI ATF
Phillips 66 Kendall® DEXRON®-VI ATF

WCHEV041 / 74656

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.