MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco Mechanism LPS® ISO 32 Hydraulic Oil
Categories: Fluid; Lubricant

Material Notes: Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor parts in heavy duty service.

Applications

Chevron Mechanism LPS Hydraulic Oils are high performance hydraulic oils recommended for use in all circulating oil systems providing power for hydraulics or hydraulic motors in heavy duty service.

Chevron Mechanism LPS hydraulic Oils have Vickers 35VQ25 vane pump approval and meet the requirements of:

  • DIN 51 524 (HVLP) gear test
  • FZG test load stage 10 (ISO 32, 46, 68)
which demonstrates outstanding pump protection under the most severe conditions.

Do not use in high pressure systems in te vicinity of flames, sparks and hot surfaces. Use only in well-ventilated areas keep container closed.

Key Words: CPS Number: 255687; MSDS Number: 7580
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 33.1 °
Viscosity Measurement 153Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 155 SUS
Saybolt Viscosity at 210°F 46.6 SUS
Kinematic Viscosity at 40°C (104°F) 30.4 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 6.1 cStASTM D445
Oxidative Stability >= 6000 hourHours to 2.0 mg KOH/g acid number; ASTM D943
 
Thermal PropertiesOriginal ValueComments
Pour Point -48.0 °CASTM D97
Flash Point 220 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Zinc, Zn 0.042 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco Mechanism LPS® ISO 15 Hydraulic Oil

WCHEV084 / 74699

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.