MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PBI Performance Products Celazole® TF-60 V Glass Fiber Reinforced Melt Processable Polybenzimidazole
Categories: Polymer; Thermoplastic; Polybenzimidazole (PBI)

Material Notes: Celazole® polybenzimidazole (PBI) resin is a unique and highly stable linear hetrocyclic polymer. PBI is characterized by high strength; excellent thermal stability, and broad chemical resistance. Celazole® T-Series products combine the superior mechanical properties and thermal resistance of PBI with the melt process ability of polyaryletherketones.
Designed for injection molding and extrusion
TF-60V is a glass-reinforced blend offering thermal and electrical insulation, wear resistance and dimensional stability with the cost efficiency of a direct form process. An excellent choice for high temperature electrical insulators, plasma torch drag cup shields, swirl baffles and parts requiring minimal thermal expansion.

Information provided by PBI Performance Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/cc
Water Absorption 0.25 %
@Temperature 22.8 °C,
Time 86400 sec
ASTM D570
Moisture Absorption at Equilibrium 4.6 %ASTM D570
Loss On Ignition 5.0 %
@Temperature 607 °C
Air; ASTM TGA
 5.0 %
@Temperature 635 °C
Nitrogen; ASTM TGA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 30ASTM D785
Tensile Strength 150 MPaASTM D638
Elongation at Break 1.4 %
Tensile Modulus 12000 MPa
Flexural Strength 225 MPaASTM D790
Flexural Modulus 12500 MPa
Compressive Strength 220 MPaASTM D695
Compressive Modulus 3600 MPa
Poissons Ratio 0.34
Shear Modulus 4.48 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.9
@Frequency 1000 Hz
ASTM D150
 3.9
@Frequency 10000 Hz
ASTM D150
Dielectric Strength 16.0 kV/mmASTM D149
Dissipation Factor 0.0010
@Frequency 10000 Hz
ASTM D150
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 25.0 - 150 °C
ASTM TMA
Specific Heat Capacity 0.270 BTU/lb-°F
@Temperature 70.0 °C
ASTM D648
Thermal Conductivity 2.50 BTU-in/hr-ft²-°F
@Temperature 23.9 °C
ASTM F-433
Deflection Temperature at 1.8 MPa (264 psi) 310 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PBI Performance Products Celazole® TU-60 Unreinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® TF-60 C Carbon Fiber Reinforced Melt Processable Polybenzimidazole
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
PBI Performance Products Celazole® TL-60 Self Lubricating Melt Processable Polybenzimidazole
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed

PPBIP004 / 140558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.