MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nylene® Nylene NX4747 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 10% Glass Fiber Filled

Material Notes: Heat stabilized nylon copolymer with 14% glass fiber reinforcement. Developed to have excellent light transmittance combined with high strength, stiffness, and resistance to automotive type fluids. Suitable for such uses as under-the-hood fluid reservoirs. Maximum clarity is achieved by using low mold temperatures.

Testing conducted on dry as molded specimen at 73°F

Information provided by Nylene® Global Polymer Solutions.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 124 MPa18000 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D638
Flexural Modulus 5.31 GPa770 ksiASTM D790
Izod Impact, Notched 0.700 J/cm1.31 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 210 °C410 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 188 °C370 °FASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Nylatron™ NSM PA6 Nylon, Cast Solid Lubricant Filled, Type 6
Ensinger TECAST VEKTON™ 6PB Nylon 6 (PA6)

PNYLEN988 / 221520

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.