MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Leaded Semi-Red Brass (Valve Metal), UNS C84400, M02 Temper, As Centrifugal Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: As Centrifugal Cast

Casting Characteristics: High – Casting Yield, Effect of Section Size; Medium – Drossing, Fluidity, Gassing, Shrinkage in Solidification

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing; Fair Suitability – Coated Metal Arc Welding

Typical uses: Ornamental Fixtures; Cases for Dead Bolt Locks; Dead Bolt Locks; Door Hardware for Prisons; Hardware; Cooling Equipment; Heating Equipment; Musical Instruments; Electrical Equipment; Low Pressure Fittings; Pump Fixtures; Valve Bodies for the Water Industry; Valve Seat; Valves; Valves for Water Meters; Boat Parts; Marine Hardware; Nuts for Transducers; Fixtures; Pipe Fittings

Applicable Specifications: As Centrifugal Cast - Castings ASTM B271/B271M; As Continuous Cast –Castings ASTM B505/B505M; As Sand Cast – Castings ASTM B584, ASTM B763/B763M; Fitting – ASME B16.32, ASME B16.18, ASME B16.24, ASME B16.23, ASME B16.15, ASTM B584, ASME B16.26; Ingot - ASTM B30; Unions – FEDERAL WW-U-516

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.69 g/cc0.314 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 200 MPa>= 29000 psifor Standard
Tensile Strength, Yield >= 89.6 MPa>= 13000 psifor Standard, 0.5% Ext
Elongation at Break >= 18 %>= 18 %for Standard
Tensile Modulus 89.6 GPa13000 ksi
Machinability 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000105 ohm-cm0.0000105 ohm-cm16.4% IACS
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 6.02 W/m-K41.8 BTU-in/hr-ft²-°F
Melting Point 842.8 - 1000 °C1549 - 1840 °F
Solidus 842.8 °C1549 °F
Liquidus 1000 °C1840 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.25 %<= 0.25 %
Copper, Cu 78 - 82 %78 - 82 %
Iron, Fe <= 0.40 %<= 0.40 %
Lead, Pb 6.0 - 8.0 %6.0 - 8.0 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 2.3 - 3.5 %2.3 - 3.5 %
Zinc, Zn 7.0 - 10 %7.0 - 10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC84400x1 / 293150

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.