MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Novodur® M203FC ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Novodur HD M203FC is an injection molding grade especially suitable for medical applications providing high flowability.

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0070 in/inISO 294-4
Melt Flow 31 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 105 MPaISO 2039-1
Tensile Strength, Yield 46.0 MPaISO 527
Elongation at Yield 2.6 %ISO 527
Tensile Modulus 2400 MPaISO 527
Flexural Strength 70.0 MPaISO 178
Flexural Modulus 2400 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 110 kJ/m²
@Temperature 23.0 °C
ISO 179
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.50 mm
Short Time; IEC 60243-1
Dissipation Factor 0.0050
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CISO 75
Vicat Softening Point 99.0 °C
@Load 5.10 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CISO 294
Mold Temperature 70.0 °CISO 294
Injection Velocity 240 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos ABS Lustran® M203FC
INEOS Styrolution Luran® S 778T ASA
Delrin Delrin® SC655 NC010 POM
INEOS Styrolution Terlux® 2802 Transparent MABS
Covestro Makrolon® LED2245 Polycarbonate

PLANX520 / 159668

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.