MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SSAB Tunnplat Domex® 044 BOR Rolled Boron Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron steels are used for a wide variety of applications - as a wear material and as a high-strength structural steel. Examples include wear plate, screen plate, punching tools, spades, knives, saw blades, caterpillar tracks, and agricultural machinery.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Estimated by MatWeb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 180180HV10; approximate
Tensile Strength, Ultimate 620 MPa89900 psi
Tensile Strength, Yield 380 MPa55100 psi
Elongation at Break 24 %24 %A5
 
Component Elements PropertiesMetricEnglishComments
Boron, B 0.0030 %0.0030 %
Carbon, C 0.25 - 0.30 %0.25 - 0.30 %
Chromium, Cr 0.40 - 0.60 %0.40 - 0.60 %
Iron, Fe 97 %97 %As Remainder
Manganese, Mn 1.0 - 1.3 %1.0 - 1.3 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si 0.20 - 0.35 %0.20 - 0.35 %
Sulfur, S <= 0.025 %<= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SSAB Tunnplat Domex® 014 BOR Rolled Boron Steel
SSAB Tunnplat Docol® 1200 DP High-strength Steel
SSAB Tunnplat Domex® 044 BOR Oil quenched Boron Steel
SSAB Tunnplat Domex® 044 BOR Water quenched Boron Steel
SSAB Tunnplat Domex® 014 BOR Water quenched Boron Steel

NTUNN90 / 19582

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.