Product Description: PPH008 is a low melt flow rate homopolymer resin that provides high melt strength and resistance to softening at elevated temperature. Typical applications include automotive and industrial applications. Availability: North America Features: Good Heat Resistance; High Melt Strength; Homopolymer; Low Flow Uses: Automotive Applications; Industrial Applications Information provided by Osterman & Company |