- By the innovative surface treatment technology, ET series has a water repellent effect.
- It is able to blend readily in W/O emulsion cream formulation.
- The inside porous structure was maintained underneath the surface coatings. Thus this product retains a moisture absorbing function which is a feature of silica gel.
Information provided by AGC Chemicals Americas Inc. |