MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break >= 200 %>= 200 %ISO 527
Flexural Modulus 1.05 GPa152 ksiISO 178
Charpy Impact, Notched  0.130 J/cm²
@Temperature -20.0 °C
0.619 ft-lb/in²
@Temperature -4.00 °F
ISO 179
 0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C120 °FISO 75
Vicat Softening Point 130 °C266 °FISO 306
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4820WZ Polypropylene, Impact Copolymer
AISI 316 Cast Stainless Steel, SUS316 Hot Formed
Permabond 935 Cyanoacrylate
Versalis KOBLEND PCA PD 935 G2 PC+ABS, 10% Glass Fiber
Unipetrol PP MONSTEN® GB 506 Polypropylene Impact Copolymer

PUNIP038 / 82898

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.