MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton 607(E) HTS-220 Synthetic Lubricating Fluid
Categories: Fluid; Lubricant

Material Notes:
  • Wide temperature range
  • Biodegradable
  • 100% synthetic
  • Minimal residue
  • Low evaporation rate
  • High flash point
  • Non-carbonizing
  • Non-oxidizing
Chesterton® 607(E) HTS-220 Lubricating Fluid is a high quality synthetic lubricant designed to provide lubrication at a wide temperature range where petroleum lubricants are unable to function. 607(E) HTS-220 Lubricating Fluid will allow the equipment to run cooler and more efficiently due to the low evaporation rate.

Chesterton 607(E) HTS-220 Lubricating Fluid is specialized for lubrication of equipment operating at elevated temperatures such as oven chains, motors, anti-friction bearings, paint curing and drying ovens, low loading gear boxes, ceramic ovens, and other high temperature equipment as well as low temperature applications in refrigerated or winter conditions.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Viscosity Measurement >= 81>= 81Index; ASTM D2270, ISO 2909
Kinematic Viscosity at 40°C (104°F) 216 cSt216 cStASTM D445, DIN 51 561
Kinematic Viscosity at 100°C (212°F) 17 cSt17 cStASTM D445, DIN 51 561
Evaporation Loss 4.62 %
@Temperature 204 °C,
Time 79200 sec
4.62 %
@Temperature 399 °F,
Time 22.0 hour
ASTM D2595
 
Mechanical PropertiesMetricEnglishComments
Four Ball Wear 0.390 mm
@Temperature 75.0 °C,
Time 3600 sec
0.0154 in
@Temperature 167 °F,
Time 1.00 hour
1200 rpm, 40 kg, scar diameter; ASTM D4172
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 255 °C491 °F
Minimum Service Temperature, Air -25.0 °C-13.0 °F
Pour Point -30.0 °C-22.0 °FASTM D97, ISO 3016
Flash Point 275 °C527 °FCOC; ASTM D92, ISO 2592
 
Descriptive Properties
AppearanceYellow/Amber
Fire Point307°CCleveland Open Cup
ISO VG220ASTM D 445

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS076o / 239863

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.