MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).

Features: High moisture vapor transmission, good low temperature properties and elasticity.

Uses: Blown and flat die/cast film extrusion.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Water Vapor Transmission 650 g/m²/day
@Temperature 23.0 °C
50% RH, Upright Cup, Water; ASTM E96B
 6000 g/m²/day
@Temperature 38.0 °C
98% RH, Upright Cup, Water; MOCON
 9500 g/m²/day
@Temperature 38.0 °C
90% RH, Upright Cup, Desiccant; ASTM E96E
Melt Flow 54 g/10 min
@Load 8.70 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength, Ultimate 4000 psiASTM D412/D638
Elongation at Break 800 %ASTM D412/D638
Tensile Modulus 0.0138 GPa500%; ASTM D412/D638
100% Modulus 0.00410 GPa
@Strain 100 %
ASTM D412/D638
300% Modulus 0.00690 GPa
@Strain 300 %
ASTM D412/D638
Tear Strength 95.0 pliSplit Tear Resistance; ASTM D470
 390 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 81
@Load 1.00 kg
H-18 wheel; ASTM D3389 B
Compression Set 17 %
@Load 0.0000224 kg,
Temperature 23.0 °C
ASTM D395
Tensile Set 10 %200% elongation; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 68.0 °CASTM D1525
 
Processing PropertiesOriginal ValueComments
Zone 1 166 - 177 °CExtrusion
Zone 2 170 - 182 °CExtrusion
Zone 3 177 - 188 °CExtrusion
Zone 4 182 - 193 °CExtrusion
Adapter Temperature 182 - 193 °CExtrusion
Die Temperature 177 - 188 °CZone 2, Extrusion
 182 - 193 °CZone 1, Extrusion
Screw Speed 15 - 40 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol Estane® MVT 75AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Lubrizol Estane® MVT 90AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission
Lubrizol Advanced Materials Pearlthane® MB-51UV Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® MB-9010 Thermoplastic Polyurethane Elastomer

PNOVEON594 / 121485

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.