MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper, UNS C15720, 24 mm rod, 0% Cold Worked
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent cold workability. Fabricated by extrusion, drawing, rolling, impacting, heading, swaging, bending, machining, blanking.

Applications: relay and switch springs, lead frames, contact supports, heat sinks, circuit breaker parts, rotor bars, resistance welding electrodes and wheels, connectors, high strength high temperature parts.

Test specimen: rod - 24mm diameter; 0% cold worked.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.81 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7474
Tensile Strength, Ultimate 470 MPa68200 psi
Tensile Strength, Yield 365 MPa
@Strain 0.2 %
52900 psi
@Strain 0.2 %
Elongation at Break 19 %19 %in 50 mm.
Modulus of Elasticity 113 GPa16400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000194 ohm-cm
@Temperature 20.0 °C
0.00000194 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.6 µm/m-°C
@Temperature 20.0 - 300 °C
10.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 353 W/m-K2450 BTU-in/hr-ft²-°F
Melting Point <= 1080 °C<= 1980 °F
Solidus 1083 °C1981 °F
Liquidus 1080 °C1980 °F
Annealing Point 649 - 982 °C1200 - 1800 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 650 - 925 °C1200 - 1700 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.35 - 0.45 %0.35 - 0.45 %
Copper, Cu 99.49 - 99.6 %99.49 - 99.6 %Specified
Iron, Fe <= 0.010 %<= 0.010 %
Lead, Pb <= 0.010 %<= 0.010 %
Oxygen, O <= 0.040 %<= 0.040 %Excluding Al2O3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
Copper, UNS C27000 (Yellow brass), OSO25 Temper flat products
Copper, UNS C26800 (Yellow brass), OSO50 Temper flat products
Copper, UNS C26800 (Yellow brass), OSO35 Temper flat products
Copper, UNS C26800 (Yellow brass), OSO25 Temper flat products

MC15720b7 / 10688

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.