MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polyram RamTal PM1409 Acetal, PTFE Filled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, PTFE Filled

Material Notes: Polyacetal filled with PTFE for sliding parts, low friction and improved wear resistance in molded parts.

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccDIN 53479
Water Absorption 0.22 %DIN 53495
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 70ASTM-D785
Tensile Strength, Yield 45.0 MPaASTM-D638
Elongation at Break 20 %ASTM-D638
Tensile Modulus 2.20 GPaASTM-D790
Flexural Strength 65.0 MPaASTM-D790
Flexural Modulus 1.75 GPaASTM-D790
Izod Impact, Notched 0.550 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmDIN 53482
Surface Resistance 1.00e+14 ohmDIN 53482
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °C
Deflection Temperature at 0.46 MPa (66 psi) 155 °CDIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 120 °CDIN 53461
Flammability, UL94 HB
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Azoty Tarnow™ TARNOFORM 500 GF6 POM
Overview of materials for Acetal Copolymer, PTFE Filled
Azoty Tarnow™ TARNOFORM 300 GF7 POM
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM
Celanese Celcon® MT24F02 Acetal Copolymer

PPOLYRA105 / 57367

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.