Sanicro 28 is a highalloy multipurpose austenitic stainless steel for service in highly corrosive conditions. The grade is characterized by:- Very high corrosion resistance in strong acids
- Very good resistance to stress corrosion cracking (SCC) and intergranular corrosion in various environments
- High resistance to pitting and crevice corrosion
- Good weldability
Information provided by Sandvik |