MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BYK Fluacolor® NS Clay
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes:
  • Fulacolor NS is a high performance reactive acid clay, produced using advanced acid activation and surface modification technology to offer a highly cost effective performance option.
  • Fulacolor NS is compatible with all capsule technologies to produce a high definition instantaneous image. Low coarse particle content minimizes abrasion and capsule bleed, and extends filter-cycles.
  • Fulacolor NS is a non-toxic material produced from natural material and consequently has extremely low environmental impact.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.441 g/cc0.0159 lb/in³aerated
 0.601 g/cc0.0217 lb/in³tapped
Particle Size 4.2 - 5.0 µm4.2 - 5.0 µmMean
pH 6.0 - 8.06.0 - 8.02% suspension in water
Viscosity <= 180 cP<= 180 cP40% solids @ pH
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 5.0 - 11 %5.0 - 11 %
 
Descriptive Properties
Whiteness>86%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BYK Cloisite® 30B Nanoclay
BYK Cloisite® 30B Bentonite
BYK Cloisite® 25A Nanoclay
BYK Cloisite® 20A Nanoclay
BYK Cloisite® 20 Salt with bentonite

PBYK043 / 185040

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.