MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Honeywell Tetrahydrofuran UV, B&J Brand® Contains No Preservative
Categories: Fluid

Material Notes: Suggested Application(s): HPLC, GC, Spectrophotometry

Product Number : Package Size : Container Type
340-1L : 6x1L : glass bottle
340-4 : 4x4L : glass bottle
NS340-20 : 20L : steel NOWPAK

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.888 g/cc
Moisture Absorption <= 0.030 %Karl Fischer Titration
Viscosity 0.55 cP
Molecular Weight 72.11 g/mol
Vapor Pressure 142 torr
Surface Tension 26.4 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Melting Point -108.5 °C
Boiling Point 66.0 °C
Flash Point -14.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4065 - 1.4075
 
Descriptive Properties
Content<2 mg/LPeroxides (as H2O2) at time of packaging

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Honeywell Tetrahydrofuran
BASF Tetrahydrofuran (THF)
Honeywell Tetrahydrofuran Purified Plus® Contains BHT Preservative
Tetrahydrofuran (THF), C4H8O
LyondellBasell THF Tetrahydrofuran

PHONWL334 / 179879

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.