MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Astryn 73A6-3 Polypropylene Copolymer, 30% Calcium Carbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, excellent chemical resistance, excellent aesthetics, high gloss, good colorability, very good processability

Applications: ABS replacement, lawn mower decks, lawn and garden tools, appliance housings

Description: Astryn 73A6-3 medium high melt flow, 30% calcium carbonate-filled polypropylene copolymer has an excellent combination of properties, chemical resistance, aesthetics and processability.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D792B
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 78ASTM D785
Tensile Strength, Ultimate 17.0 MPaASTM D638
Tensile Strength, Yield 18.0 MPaASTM D638
Elongation at Break 350 %ASTM D638
Elongation at Yield 6.0 %ASTM D638
Flexural Modulus 1.20 GPaTangent at 0.05 in/min; ASTM D790A
Izod Impact, Notched 1.20 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 83.0 °CASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ Q 100 F Polyolefin
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability
LG Chemical LUMAX IN-5001 High Impact PBT
LyondellBasell Adflex™ KS-021P TPO Resin
LyondellBasell Astryn 75A6-2 Polypropylene Copolymer, 20% Calcium Carbonate

PMO348 / 53605

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.