LNP THERMOCOMP Z1C00VI compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing proprietary fillers. Added features of this grade include: Ultra-Low Dielectric Constant and Loss Tangent for Laser Direct Structuring (LDS), High HDT, Low Warpage, Excellent Surface Finishing and Chemical Resistant. Features: Chemical Resistance,Enhanced Chemical Resistance,High Heat Resistance,Laser Direct Structuring,Circuit Solution,Low Warpage Information provided by SABIC |