MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Trigonox 41-C50 tert-Butyl peroxyisobutyrate
Categories: Other Engineering Material

Material Notes: Initiator (50% active ingredient in odorless mineral spirits) for (co)polymerization of ethylene and styrene.

CAS number: 109-13-7

EINECS/ELINCS No: 203-650-5

Applications: Trigonox 41-C50 is an efficient initiator for the ethylene polymerization under high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, combinations with other peroxides are applied in practice. Depending on reaction conditions, Trigonox 41-C50 is active in the temperature range between 165°C and 250°C.Trigonox 41-C50 can be used for the polymerization of styrene in the temperature range between 85°C and 105°C. Main application is the copolymerization of styrene with acrylonitrile, acrylates and methacrylates.Trigonox 41-C50 can be used as initiator for the solution (co)polymerization of acrylates and methacrylates in the temperature range of 80- 160°C, amongst others for the manufacture of coatings.Trigonox 41-C50 can also be applied as an initiator for the bulk and suspension (co)polymerization of acrylates and methacrylates.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.840 g/cc
@Temperature 10.0 °C
0.0303 lb/in³
@Temperature 50.0 °F
Storage Temperature <= 10.0 °C<= 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 30.0 °C86.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay49.0-51.0 %
Color=20 Pt-Co
Content=0.10 %Hydroperoxides as TBHP
 =100 mg/kgInorganic + organic hydrolysable chloride
 4.89-5.09 %Active oxygen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1112 / 286635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.