MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 949 Series, Conductive Sanding Gel Coat
Categories: Polymer; Thermoset

Material Notes: POLYCOR® 949 Series sanding gel coats have been specifically formulated for use as a sanding substrate. Sanding gel coats are used for FRP parts that will be subsequently painted. They can be used for room temperature and heated molding (RTM) applications. Customer experiences have proven that these products can be post-baked at temperatures up to 285°F for as long as two hours. They may also be used for utility, noncritical exterior applications. They are not intended (nor should they be used) as a surface coat for the marine, tub/shower or swimming pool industries. They should not be used for water immersion service (boat hull, swimming pool, spa, water tank, etc.), even if/when painted.

Features and Benefits:

  • Easy to spray
  • Resistance to porosity and pinholing
  • Easy to sand when cured

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 11000 - 20000 cP11000 - 20000 cPRVF #4 spindle @ 4 rpm
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 50000 ohm50000 ohm
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min0.750 - 1.00 hourLay-up Time
Gel Time 4.00 - 22.0 min
@Temperature 25.0 °C
4.00 - 22.0 min
@Temperature 77.0 °F
100 g mass, 77°F, 1.8% or 2% Arkema Luperox® DDM-9
 
Descriptive Properties
Sag ResistanceGood @ 20 mils
Thixotropic Index5.5-72/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9217 / 231812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.