MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SK Chemicals SKYPET® BR-V Semi-crystalline Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: SKYPET® BR is a semi-crystalline copolyester grade with excellent transparency, chemical resistance, and processability. Due to its slower crystallization rate compared to a regular PET, BR is suited for making thicker products for variety of applications through injection, stretch blow molding, and sheet extrusion processing. SKYPET® BR does not contain Bisphenol derivatives (BPA, etc.) and Phthalate-based plasticizer components regulated by the EU RoHS regulations. It also meets the requirements for food contact materials in Korea, the US, Europe, China, and Japan.

Applications: 5-gallon mineral water bottles. Containers for cosmetics. Sheet (outer packing and wrapping materials): excellent thermoforming, enabling deep draw. Thickness of thermoforming, 5 or 6 mm. Returnable bottles.

Attributes: Not easily crystallized compared to SKYPET BB and SKYPET BL. More easily applicable when forming thick materials compared to SKYPET BB and SKYPET BL. Transparency is ensured Requires lower temperature for formation than SKPET BB and SKYPET BL. Minimal occurrence of byproducts, such acetaldehyde.

Information provided by SK Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D785
Tensile Strength at Break 21.6 MPaASTM D638
Tensile Strength, Yield 51.0 MPaASTM D638
Elongation at Break 250 %ASTM D638
Elongation at Yield 4.5 %ASTM D638
Flexural Strength 75.5 MPaASTM D790
Flexural Modulus 2220 MPaASTM D790
Izod Impact, Notched 51.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
UV Transmittance 89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSK9927 / 291443

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.