MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

CHT CHT-BeauSil™ AMO 804 Modified siloxane
Categories: Other Engineering Material

Material Notes: Description: Amodimethicones are functionalized silicones with nitrogen groups. These modification improves the deposite and the affinity to the hair. Amodimethicones are showing excellent combing and a good gloss on hair. These silicone polymers are ideal for all kind of hair care application were best performance is needed.

Key Features

  • Improves combing behaviour
  • Smoothness
  • Improves Gloss
  • Heat and Color protection
Key Applications
  • Hair Care
  • Treatments
  • Conditioner
  • Rinse-off products
Application: CHT-BeauSil™ AMO 804 is a fluid of an amino siloxane used in hair care applications. By the high viscosity of CHT-BeauSil™ AMO 804 it gives a very soft and nice feeling to the hair. It gives repairing properties as well as heat and color protection.

Addition Rates
Dosage - 1: 0.3 - 3.0% in rinse-off products
Dosage - 2: 0.1 - 2.0% in leave-on products
Dosage - 3: 0.5 - 5.0% in treatments

INCI Name: Amodimethicone

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 0.00 %0.00 %
Brookfield Viscosity 1000 - 6000 cP1000 - 6000 cP
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Nitrogen, N 0.40 %0.40 %
 
Descriptive Properties
AppearanceColorless to yellow liquid
IonicityCationic
MIT FreeYes
Ultralow cyclic contentNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL201 / 314684

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.