MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Corr-Paint™ CP4000-S1-HT High Temperature Silicone Protective Coating
Categories: Polymer; Thermoset; Silicone

Material Notes: Aremco’s Corr-Paint™ CP40xx-S1 series coatings are formulated using an advanced solvent-based silicone resin combined with inorganic fillers and pigments to offer continuous temperature resistance to 1100°F (593°C) and intermittent resistance to 1200°F (649°C). A higher temperature formulation, CP4000-S1-HT, offers continuous operation to 1400°F (593°C) and intermittent resistance to 1800°F (982°C). These coatings are single-part, heat curable systems that adhere to a wide range of materials including metals, ceramics, glass, quartz, and refractories, and offer outstanding resistance to outdoor weathering, UV light, salt spray corrosion, oxidation, some chemicals, and thermal shock.

Product Highlights

  • Single-Part, No Mixing
  • Low Viscosity
  • Maximum Use Temperature, 1100–1400 °F (593–760 °C)
  • Good Chemical Resistance
  • Bonds to Ceramics, Glass, Quartz, Metals
  • Excellent Resistance to Moisture & Salt Spray
  • Resists Thermal Shock
  • Resists Ultraviolet Light
  • Solvent-Based
Typical Applications
  • Bag Houses
  • Boiler Casings
  • Chimneys
  • Cyclones
  • Ducting
  • Heaters
  • Heat Exchangers
  • Exhaust Systems
  • Engines
  • Furnaces, Ovens, Kilns
  • Lighting Fixtures
  • Process Vessels
  • Reformers
  • Scrubbers
  • Stacks
  • Turbochargers

Vendors: Aremco offers a broad range of coatings formulated using an advanced solvent-based silicone resin combined with inorganic fillers and pigments. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.61 g/cc1.61 g/cc
Solids Content 53.6 %53.6 %Volume
 79 %79 %Weight
Volatiles 29 %29 %
Viscosity 900 - 1200 cP900 - 1200 cP
Thickness 1.00 microns0.0394 milDry Film Thickness
 1.90 microns0.0748 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 760 °C1400 °F
Flash Point 47.8 °C118 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 32.2 °C40.0 - 90.0 °FApplication Temperature
Dry Time >= 1.00 hour>= 1.00 hourCuring, Min Air Set
 1.00 - 2.00 hour1.00 - 2.00 hourTouch
 2.00 - 4.00 hour2.00 - 4.00 hourHandling
 1.00 - 24.0 hour1.00 - 24.0 hourRecoat
Cure Time  15.0 min
@Temperature 93.3 °C
0.250 hour
@Temperature 200 °F
 15.0 min
@Temperature 249 °C
0.250 hour
@Temperature 480 °F
 15.0 min
@Temperature 649 °C
0.250 hour
@Temperature 1200 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBlack
Theoretical Dry Film Coverage, ft2/gal860
ThinnerPM Acetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM964 / 316324

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.