MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Conpol™ 5B10S1 Ethylene-Methacrylic Acid Additive Resin
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Compounding Grade

Material Notes: Conpol™ additive resins, supplied in pellet form, are designed to modify the surface properties of films or coatings of Surlyn® ionomer resins and Nucrel® acid copolymer resins. They are concentrated masterbatch products and should not be used by themselves in extrusion equipment, but blended with the resin to be modified. Conpol™ products are made from ethylene-methacrylic acid carrier resins to maximize compatibility with Surlyn® and Nucrel® resins.

Information provided by DuPont Packaging Polymers.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccASTM D792
Melt Flow 25 g/10 minCond. E; ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
Dow Conpol™ 20S2 Ethylene-Methacrylic Acid Additive Resin
Dow Conpol™ 4R11S1 Ethylene-Methacrylic Acid Additive Resin
Dow Elvaloy® AC 2618 Ethylene Methyl Acrylate

PDUPE0 / 33589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.