MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Bloc® Module HS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Pyro-Bloc HS Module is a unique innovation in ceramic fiber module systems. Proprietary manufacturing techniques result in enhanced mechanical abuse resistance which allows Pyro-Bloc HS to be installed in applications never before thought possible with ceramic fiber of any type. Like all Pyro-Bloc products, Pyro-Bloc HS starts with Pyro-Log fiber which possesses the unique ability to become extremely hard after burnout of the organic lubricant. This benefit is enhanced by the addition of a proprietary hardening agent during manufacturing ensuring full and homogeneous penetration.

Applications:

  • Stack linings
  • Flare linings
  • Ductwork linings
  • Kiln car block
  • Kiln car seals
  • Burner block
  • Peep sights
  • Corbell block
  • Convection section
  • Fluidized bed units

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.368 g/ccfired
 0.481 g/ccfired
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0800 W/m-K
@Temperature 260 °C
ASTM C201
 0.140 W/m-K
@Temperature 538 °C
ASTM C201
 0.230 W/m-K
@Temperature 816 °C
ASTM C201
 0.320 W/m-K
@Temperature 1093 °C
ASTM C201
Melting Point 1650 °C
Maximum Service Temperature, Air 1093 °CContinuous Use
 1204 °C
 
Descriptive Properties
Colorwhite/pale green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax PC Series™ PC Max™ Paper Ceramic Fiber Filtration Media
Saint-Gobain Chemfab® TCN® 1590 Leno Weave Nomex/Fiberglass Belting Material
Pyrotek Grade 1250 Ceramic fiber paper
Morgan Advanced Ceramics Thermo-Bloc Modules Ceramic Fiber Thermal Ceramic
Morgan Advanced Ceramics Pyro-Bloc® EES System R Thermal Ceramic

CMORF70153 / 203451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.