MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mullite, 3Al2O3-2SiO2
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes:

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.80 g/ccASTM C20
Water Absorption 0.00 %ASTM C373
 
Mechanical PropertiesOriginal ValueComments
Knoop Microhardness 1450kg/mm²
Hardness, Rockwell 45 N 70
Modulus of Elasticity 150 GPaASTM C848
Flexural Strength 170 MPaASTM F417
Compressive Strength 550 MPaASTM C773
Poissons Ratio 0.25ASTM C848
Shear Modulus 60.0 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cmASTM D1829
 300000 ohm-cm
@Temperature 1000 °C
ASTM D1829
 5.00e+12 ohm-cm
@Temperature 500 °C
ASTM D1829
Dielectric Constant 6.5
Dielectric Strength 9.80 kV/mmASTM D116
Dissipation Factor 0.0020ASTM D2520
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°C
@Temperature 20.0 °C
 5.00 µm/m-°C
@Temperature 250 °C
 5.00 µm/m-°C
@Temperature 500 °C
 5.30 µm/m-°C
@Temperature 1000 °C
ASTM C372
Specific Heat Capacity 0.950 J/g-°CASTM E1269
Thermal Conductivity 3.50 W/m-KASTM C408
Melting Point 1880 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.64
IR Transmittance 85 %
@Thickness 0.220 mm
cutoff is 4.8 µm.
 
Processing PropertiesOriginal ValueComments
Sintering Temperature 1620 °C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Zirconium Oxide, Zirconia, ZrO2
Cordierite, 2MgO-2Al2O3-5SiO2
Germanium Mullite, 3Al2O3-2GeO2
Yttria Stabilized Zirconia, YSZ

BMULL0 / 250

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.