MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BRP Manufacturing BG618 – Style 5368 Nitrile Rubber Sheet, Peroxide Cure
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Material: Nitrile Rubber Sheet, Peroxide Cure
BRP Style: BG618 – Style 5368
Finish: Smooth (nylon available)
ASTM Callout: ASTM D2000 2BG618EO14EO34F16Z1Z2Z3Z4, Z1 = BRP Style 5368, Z2 Peroxide Cure Nitrile, Z3 = Compression Set 35% Max. (D395, 100°C), Z4 = Conforms to WH 45351EZ and GE A12C11E7

Information provided by BRP Manufacturing Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 12.4 MPa>= 1800 psiOriginal; ASTM D412
 <= 6.83 MPa
@Temperature 100 °C,
Time 252000 sec
<= 990 psi
@Temperature 212 °F,
Time 70.0 hour
EO34, IRM 903 Oil; ASTM D471
 <= 9.31 MPa
@Temperature 100 °C,
Time 252000 sec
<= 1350 psi
@Temperature 212 °F,
Time 70.0 hour
EO14, IRM 901 Oil; ASTM D471
 <= 9.93 MPa
@Temperature 100 °C,
Time 252000 sec
<= 1440 psi
@Temperature 212 °F,
Time 70.0 hour
Heat Resistance; ASTM D573
 9.93 - 14.9 MPa
@Temperature 100 °C,
Time 252000 sec
1440 - 2160 psi
@Temperature 212 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Elongation at Break 270 %270 %Original; ASTM D412
 <= 148.5 %
@Temperature 100 °C,
Time 252000 sec
<= 148.5 %
@Temperature 212 °F,
Time 70.0 hour
EO14, IRM 901 Oil; ASTM D471
 <= 148.5 %
@Temperature 100 °C,
Time 252000 sec
<= 148.5 %
@Temperature 212 °F,
Time 70.0 hour
EO34, IRM 903 Oil; ASTM D471
 <= 162 %
@Temperature 100 °C,
Time 252000 sec
<= 162 %
@Temperature 212 °F,
Time 70.0 hour
Heat Resistance; ASTM D573
 <= 202.5 %
@Temperature 100 °C,
Time 252000 sec
<= 202.5 %
@Temperature 212 °F,
Time 70.0 hour
Heat Aged; ASTM D573
Compression Set  <= 35 %
@Temperature 100 °C,
Time 79200 sec
<= 35 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395 Method B
 <= 50 %
@Temperature 100 °C,
Time 79200 sec
<= 50 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395 S
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 100 °C212 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Descriptive Properties
Hardness50-65EO34, IRM 903 Oil, 70 h @ 100°C, ASTM D471
 55-75Heat Aged, ASTM D573, 70 h @ 100°C
 55-75Heat Resistance, D573, 70 hours @ 100°C
 60-70ASTM D2240
 60-80EO14, IRM 901 Oil, 70 h @ 100°C, ASTM D471
Oil Immersion<40% Volume ChangeASTM D471, IRM 903 Oil, 70 h @ 100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBRPM030 / 315691

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.