MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Diisopropanol-p-toluidine
Categories: Fluid

Material Notes: Formula: C13H21NO2

CAS: 38668-48-3

Description: Diisopropanol-p-toluidine is a colorless to yellowish paste with and amine-like odor. This product is only sparingly soluble in water.

Synonyms: DIIPT, N,N-Bis(2-hydroyxpropyl)-p-toluidin

Applications: This product is used as a polymerization initiator in synthetic resin systems

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cc
Molecular Weight 223.3 g/mol
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 - 72.0 °C
Boiling Point >= 300 °C
Flash Point 175 °C
Ignition Temperature 290 °C
 
Descriptive Properties
Assay>97%
CompositionDiisopropanol-p-toluidine(over propoxilated)<3.5%
 Monisopropanol-p-toluidine<1.0%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Dicykan 4,4'-Diaminodicyclohexylmethane
BASF AH-Salt
BASF Ethyl-(2-hydroxyethyl)aniline
BASF Ethylene Carbonate S
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe)

PBASG0911 / 132544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.