MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese SO.F.TER Talcoprene® 340TL Talc-Reinforced Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Standard Talcoprene® 40% Talc-Reinforced Polypropylene

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
Water Absorption 0.050 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0080 - 0.012 cm/cmSO.F.TER Method
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 72ASTM D785
Tensile Strength 30.0 MPaASTM D638
Flexural Strength 49.0 MPaASTM D790
Flexural Modulus 3800 MPaASTM D790
Izod Impact, Notched 32.0 J/mASTM D256/A
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+13 ohmASTM D257
Dielectric Constant 2.5ASTM D150
Comparative Tracking Index >= 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 90.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °CASTM D648
Vicat Softening Point 95.0 °C50°C/h at 50 N; ASTM D1525
Flammability, UL94 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black
RheTech Products T30P100-01 30% Talc Reinforced Polypropylene, Black
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural
LyondellBasell Hostacom™ XFBR712 Thermoplastic Polyolefin Elastomer
LyondellBasell Hostacom™ 63A6-4 Polypropylene Homopolymer

PSOFS840 / 162304

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.