MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Materion ToughMet® 3AT, Copper-Nickel-Tin Alloy Rod AT110, 4 to 9 in
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: ToughMet 3 AT alloy is a wrought, spinodally hardened copper alloy engineered for high strength and hardness. It resists mechanical wear, galling, stress relaxation, corrosion and erosion. ToughMet 3 alloy retains its strength at elevated temperature. It is non-magnetic and easy to machine into complex components.

Information provided by Materion.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.00 g/cc0.325 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 30.030.0
Tensile Strength, Ultimate 876 MPa127000 psi
Tensile Strength, Yield 758 MPa
@Strain 0.200 %
110000 psi
@Strain 0.200 %
Elongation at Break 6.00 %6.00 %
Poissons Ratio 0.3300.330
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 0.0000250 ohm-cm>= 0.0000250 ohm-cm
Magnetic Permeability <= 1.001<= 1.001
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.4 µm/m-°C9.10 µin/in-°F
Thermal Conductivity 38.0 W/m-K264 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 77.0 %77.0 %
Nickel, Ni 15.0 %15.0 %
Tin, Sn 8.00 %8.00 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NBBC12d / 323569

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.