MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Vinnolit® P 80 PVC for Paste Application
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Vinnolit® P 80 PVC for paste application. Vinnolit® P 80 is a fine grained homopolymer for plastisol processing giving low viscosity plastisols with an excellent shelf life. Vinnolit® P 80 pastes with a medium plasticizer content show Newtonian rheology at low shear rates (Brookfield) and dilatant behavior at high shear rates. The dilatancy can readily be reduced or even eliminated by blending with extender resins such as Vinnolit® EXT or with specialty emulsion grades. Due to the very low emulsifier content this product shows very low moisture absorption and shows an excellent thermostability with high-gloss-film-finish. The main application areas are transparent top coats, special dip coating processes and for cover seals/gaskets. The core properties of Vinnolit® P 80 are: very fine particles, lowest initial viscosity, very low moisture absorption in powder, and film excellent thermostability, crystal clear films and highest, transparency, good miscibility with Extender resins and special blending grades, demi matt or highly glossy adjustable, good mechanical parameters, excellent weathering properties, very high storage stabilities, low sedimentation in thin plastisols.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.30 %
Apparent Bulk Density 0.330 g/ccISO 60
Particle Size <= 63 µm<= 1.0% Retained on 0.063 mm Sieve; DIN EN ISO 53195
Viscosity Test 1.69 dl/gReduced Viscosity; ISO 1628-2
 
Descriptive Properties
Emulsifier ContentExtremely low
K-Value80ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO926 / 291123

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.