MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPE ME-2380-01 BLK 111 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2380-01 BLK 111 is a high performance thermoplastic elastomer designed for automotive exterior molding applications. Sarlink ME-2380-01 BLK 111 is a medium hardness, low density, UV stabilized grade delivering excellent aesthetics and good injection molding cycle times.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Good Surface Finish; Low Density; Medium Hardness; Low Specific Gravity; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Handles; Rubber Replacement; Weatherstripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
20 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  80
@Time 5.00 sec
80
@Time 0.00139 hour
ASTM D2240
 83
@Time 1.00 sec
83
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 6.69 MPa970 psiFlow; ASTM D412
 12.7 MPa1840 psiAcross Flow; ASTM D412
Elongation at Break 640 %640 %Flow; ASTM D412
 850 %850 %Across Flow; ASTM D412
Tear Strength 38.6 kN/m220 pliASTM D624
Compression Set  31 %
@Temperature 22.8 °C,
Time 79200 sec
31 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ISO 815
 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ISO 815
 87 %
@Temperature 90.0 °C,
Time 252000 sec
87 %
@Temperature 194 °F,
Time 70.0 hour
Type 1; ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 216 - 227 °C420 - 440 °FMelt, Injection
Rear Barrel Temperature 199 - 210 °C390 - 410 °FInjection
Middle Barrel Temperature 204 - 216 °C400 - 420 °FInjection
Front Barrel Temperature 210 - 221 °C410 - 430 °FInjection
Nozzle Temperature 216 - 227 °C420 - 440 °FInjection
Zone 1 193 - 204 °C380 - 400 °FExtrusion
Zone 2 199 - 210 °C390 - 410 °FExtrusion
Zone 3 204 - 216 °C400 - 420 °FExtrusion
Zone 4 204 - 216 °C400 - 420 °FExtrusion
Zone 5 210 - 221 °C410 - 430 °FExtrusion
Die Temperature 216 - 227 °C420 - 440 °FExtrusion
Mold Temperature 35.0 - 65.6 °C95.0 - 150 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1074 / 237565

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.