MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman ComAlloy Hiloy® 632 Nylon 6/6, Glass Reinforced, Flow Enhanced, UL
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Data provided by the manufacturer, ComAlloy International Company.

20% Glass Reinforced.

The ComAlloy product line has been integrated into the A Schulman product line.

Key Words: Polyamide 6/6; Polyamide 66; Nylon 66; ComAlloy International Company, subsidiary of A. Shulman Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/cc
Linear Mold Shrinkage 0.0040 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Ultimate 127 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Flexural Strength 169 MPaASTM D790
Flexural Modulus 4.80 GPaASTM D790
Izod Impact, Notched 0.530 J/cmASTM D256
Izod Impact, Unnotched 5.60 J/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 255 - 275 °C
Deflection Temperature at 0.46 MPa (66 psi) 210 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 200 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 271 - 285 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy® E-16558 30% Glass Fiber Reinforced Nylon
A. Schulman ComAlloy Hiloy® 631 Nylon 6/6, Glass Reinforced, Flow Enhanced
A. Schulman ComAlloy Hiloy® 625 Nylon 6/6, Glass Reinforced
A. Schulman ComAlloy Hiloy® 622 Nylon 6/6, Glass Reinforced, UL
Asahi Kasei Leona™ 54G33 Polyamide 66, GF Reinforced

PASH12 / 24801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.